Research/Sitter/MAGNDATA / 2.60_NdMn2Si2.mcif

⬇ Download .mcif  ·  Data (JSON)

Spin lattice of NdMn2Si2Spin lattice of NdMn2Si2

NdMn2Si2

MAGNDATA entry 2.60 · source
noncollinear ferrimagnet
Opposite moments of different size leave a net magnetisation.
ordered ≤ 34 K (−239 °C)Colour: where that sits relative to 25 °C. Saturation: how much margin it has.
Structure · 10 properties
Magnetic groupP m m′ n′ BNS 59.410
Parent space groupI 4/m m m No. 139
Spinscoplanar · net moment 11.22 μB per cell
Propagation[0 0 0] · [1 1 1] 2k
Cella 3.996 · b 3.996 · c 10.478 Å · α 90° · β 90° · γ 90°
Transition34 K (−239 °C)
Measured at1.6 K
Magnetic ionsMn, Nd
Largest moment component2.83 μB
MethodNPD

Symmetry

Stereogram of the magnetic point group: each operation applied to one direction. Filled = upper hemisphere, ring = lower; red operations include time reversal. Lines are mirrors; polygons are 2/3/4/6-fold axes; the centre ring is inversion.

Every structure in P m m′ n′ →
Atom sites · 3 sites · CSV
siteelementxyzmambmc|m| (μB)
Nd1Nd000002.832.83
Mn1Mn00.50.250−0.811.391.6088
Si1Si000.3797

Moment components are along the crystal axes a, b, c (μB), as magCIF writes them. Symmetry generates the rest of the cell from these sites.

Source

R. Welter et al. Journal of Alloys and Compounds (1993) · doi:10.1016/0925-8388(93)90075-X

Cite the original paper and MAGNDATA, not this mirror.

Original file

⬇ 2.60_NdMn2Si2.mcif from MAGNDATA · entry page

sha256 of this copy: 08c2ef3d08dbcebfbce3bcad8421c713abe35c0931297d7fb2dadc3a8adf4a39
The mirror keeps the bytes Bilbao served, so the original should hash the same unless MAGNDATA has revised the entry since: shasum -a 256 2.60_NdMn2Si2.mcif.