Research/Sitter/MAGNDATA / 1.407_Nd2CuO4.mcif

⬇ Download .mcif  ·  Data (JSON)

Spin lattice of Nd2CuO4Spin lattice of Nd2CuO4

Nd2CuO4

MAGNDATA entry 1.407 · source
antiferromagnet
No net magnetisation, and up and down sublattices are related by a shift or by inversion, so the bands stay spin-degenerate: a conventional antiferromagnet.
Spin group ¹m¹m¹m × ²1: each symmetry marked ¹ keeps every spin, ² swaps up and down.
ordered ≤ 75 K (−198 °C)Colour: where that sits relative to 25 °C. Saturation: how much margin it has.
Structure · 10 properties
Magnetic groupCA m c a BNS 64.480
Parent space groupI 4/m m m No. 139
Spinscollinear · net moment 0 μB per cell
Propagation[1/2 1/2 0] 1k
Cella 7.8758 · b 7.8758 · c 12.14 Å · α 90° · β 90° · γ 90°
Transition75 K (−198 °C)
Measured at50 K
Magnetic ionsCu, Nd
Largest moment component0.28 μB
MethodNSD

Symmetry

Stereogram of the magnetic point group: each operation applied to one direction. Filled = upper hemisphere, ring = lower; red operations include time reversal. Lines are mirrors; polygons are 2/3/4/6-fold axes; the centre ring is inversion.

Every structure in CA m c a →
Atom sites · 4 sites · CSV
siteelementxyzmambmc|m| (μB)
Nd1Nd000.3512
Cu1Cu0000.28−0.2800.396
O1O00.250
O2O00.250.25

Moment components are along the crystal axes a, b, c (μB), as magCIF writes them. Symmetry generates the rest of the cell from these sites.

Source

M. Matsuda et al. PHYSICAL REVIEW B (1990) · doi:10.1103/PhysRevB.42.10098

Cite the original paper and MAGNDATA, not this mirror.

Original file

⬇ 1.407_Nd2CuO4.mcif from MAGNDATA · entry page

sha256 of this copy: 3a50b14fabc3006812ebfcf7f88a530642baaea35a8f0358e36ff5fab883e5ca
The mirror keeps the bytes Bilbao served, so the original should hash the same unless MAGNDATA has revised the entry since: shasum -a 256 1.407_Nd2CuO4.mcif.