Research/Sitter/MAGNDATA / 1.203_Ni2SiO4.mcif

⬇ Download .mcif  ·  Data (JSON)

Spin lattice of Ni2SiO4Spin lattice of Ni2SiO4

Ni2SiO4

MAGNDATA entry 1.203 · source
noncollinear antiferromagnet
All moments add up to a net magnetisation: an ordinary magnet. Spin splitting is the same in every direction (s-wave).
ordered ≤ 34 K (−239 °C)Colour: where that sits relative to 25 °C. Saturation: how much margin it has.
Structure · 10 properties
Magnetic groupPc 21/c BNS 14.82
Parent space groupP n m a No. 62
Spinscoplanar · net moment 0 μB per cell
Propagation[1/2 0 1/2] 1k
Cella 20.2346 · b 5.9125 · c 9.4554 Å · α 90° · β 90° · γ 90°
Transition34 K (−239 °C)
Measured at5 K
Magnetic ionsNi
Largest moment component1 μB
MethodNPD

Symmetry

Stereogram of the magnetic point group: each operation applied to one direction. Filled = upper hemisphere, ring = lower; red operations include time reversal. Lines are mirrors; polygons are 2/3/4/6-fold axes; the centre ring is inversion.

Every structure in Pc 21/c →
Atom sites · 12 sites · CSV
siteelementxyzmambmc|m| (μB)
Ni1_1Ni0001011.4142
Ni1_2Ni0.2500.25−1011.4142
Ni2_1Ni0.13690.250.4962−10−11.4142
Ni2_2Ni0.11310.750.746210−11.4142
Si1_1Si0.04710.250.2135
Si1_2Si0.20290.750.4636
O1_1O0.04660.250.3847
O1_2O0.20340.750.6347
O2_1O0.22260.250.1086
O2_2O0.02740.750.3586
O3_1O0.08160.03010.1372
O3_2O0.16840.96990.3872

Moment components are along the crystal axes a, b, c (μB), as magCIF writes them. Symmetry generates the rest of the cell from these sites.

Source

R.E. Newnham et al. Acta Cryst. (1965) · doi:10.1107/S0365110X6500289X

Cite the original paper and MAGNDATA, not this mirror.

Original file

⬇ 1.203_Ni2SiO4.mcif from MAGNDATA · entry page

sha256 of this copy: b229485799281c8cfd6f0c102ea568e8ad59aeed8bb690d028b025987ec60644
The mirror keeps the bytes Bilbao served, so the original should hash the same unless MAGNDATA has revised the entry since: shasum -a 256 1.203_Ni2SiO4.mcif.