Research/Sitter/MAGNDATA / 0.869_Pr2NiIrO6.mcif

⬇ Download .mcif  ·  Data (JSON)

Spin lattice of Pr2Ni1Ir1O6Spin lattice of Pr2Ni1Ir1O6

Pr2Ni1Ir1O6

MAGNDATA entry 0.869 · source
noncollinear ferrimagnet
Opposite moments of different size leave a net magnetisation.
ordered ≤ 5 K (−268 °C)Colour: where that sits relative to 25 °C. Saturation: how much margin it has.
Structure · 11 properties
Magnetic groupP 21/c BNS 14.75
Point group2/m
Parent space groupP 21/n’ No. 14
Spinscoplanar · net moment 7.28 μB per cell
Propagation[0 0 0] 1k
Cella 5.4699 · b 5.6651 · c 7.7843 Å · α 90° · β 90.05° · γ 90°
Transition5 K (−268 °C)
Measured at1.5 K
Magnetic ionsIr, Ni, Pr
Largest moment component1.54 μB
MethodNPD

Symmetry

Stereogram of the magnetic point group: each operation applied to one direction. Filled = upper hemisphere, ring = lower; red operations include time reversal. Lines are mirrors; polygons are 2/3/4/6-fold axes; the centre ring is inversion.

Every structure in P 21/c →
Atom sites · 6 sites · CSV
siteelementxyzmambmc|m| (μB)
Ni1Ni000.50.561.5401.6387
Ir1Ir000−0.2−0.3400.3945
Pr1Pr0.0120.56150.7511.011.2201.5838
O1O0.09640.02480.266
O2O0.1970.3030.9386
O3O0.1890.2810.5274

Moment components are along the crystal axes a, b, c (μB), as magCIF writes them. Symmetry generates the rest of the cell from these sites.

Source

T. Ferreira et al. PHYSICAL REVIEW MATERIALS (2021) · doi:10.1103/PhysRevMaterials.5.064408

Cite the original paper and MAGNDATA, not this mirror.

Original file

⬇ 0.869_Pr2NiIrO6.mcif from MAGNDATA · entry page

sha256 of this copy: aecd78780f9b4109172c70e303688be77414d1aef1ded7c29bc9c3e9cf181ee0
The mirror keeps the bytes Bilbao served, so the original should hash the same unless MAGNDATA has revised the entry since: shasum -a 256 0.869_Pr2NiIrO6.mcif.