Research/Sitter/MAGNDATA / 0.771_PrMnSi2.mcif

⬇ Download .mcif  ·  Data (JSON)

Spin lattice of PrMnSi2Spin lattice of PrMnSi2

PrMnSi2

MAGNDATA entry 0.771 · source
s-wave ferromagnet
All moments add up to a net magnetisation: an ordinary magnet. Spin splitting is the same in every direction (s-wave).
Spin group ¹m¹m¹m: each symmetry marked ¹ keeps every spin, ² swaps up and down.
ordered ≤ 434 K (161 °C)Colour: where that sits relative to 25 °C. Saturation: how much margin it has.
Structure · 11 properties
Magnetic groupC m′ c m′ BNS 63.464
Point groupm′m′m
Parent space groupC m c m No. 63
Spinscollinear · net moment 8.24 μB per cell
Propagation[0 0 0] 1k
Cella 4.094 · b 17.553 · c 4.028 Å · α 90° · β 90° · γ 90°
Transition434 K (161 °C)
Measured at200 K
Magnetic ionsMn, Pr
Largest moment component2.06 μB
MethodNPD

Symmetry

Stereogram of the magnetic point group: each operation applied to one direction. Filled = upper hemisphere, ring = lower; red operations include time reversal. Lines are mirrors; polygons are 2/3/4/6-fold axes; the centre ring is inversion.

Every structure in C m′ c m′ →
Atom sites · 4 sites · CSV
siteelementxyzmambmc|m| (μB)
Pr1Pr00.10230.25
Mn1Mn00.750.2502.0602.06
Si1Si00.32520.25
Si2Si00.46620.25

Moment components are along the crystal axes a, b, c (μB), as magCIF writes them. Symmetry generates the rest of the cell from these sites.

Source

B. Malaman et al. Journal of Magnetism and Magnetic Materials (1990) · doi:10.1016/0304-8853(90)90143-E

Cite the original paper and MAGNDATA, not this mirror.

Original file

⬇ 0.771_PrMnSi2.mcif from MAGNDATA · entry page

sha256 of this copy: 4a641cd7c5cae5ff46ad4db29ae90b717417372f1df0f498646275ade79c138a
The mirror keeps the bytes Bilbao served, so the original should hash the same unless MAGNDATA has revised the entry since: shasum -a 256 0.771_PrMnSi2.mcif.