Research/Sitter/MAGNDATA / 0.690_NdPt.mcif

⬇ Download .mcif  ·  Data (JSON)

Spin lattice of NdPtSpin lattice of NdPt

NdPt

MAGNDATA entry 0.690 · source
s-wave ferromagnet
All moments add up to a net magnetisation: an ordinary magnet. Spin splitting is the same in every direction (s-wave).
Spin group ¹m¹m¹m: each symmetry marked ¹ keeps every spin, ² swaps up and down.
ordered ≤ 23 K (−250 °C)Colour: where that sits relative to 25 °C. Saturation: how much margin it has.
Structure · 10 properties
Magnetic groupC 2′/c′ BNS 15.89
Parent space groupC m c m No. 63
Spinscollinear · net moment 9.367 μB per cell
Propagation[0 0 0] 1k
Cella 3.846 · b 10.769 · c 4.542 Å · α 90° · β 90° · γ 90°
Transition23 K (−250 °C)
Measured at4.2 K
Magnetic ionsNd
Largest moment component2.17 μB
MethodNPD

Symmetry

Stereogram of the magnetic point group: each operation applied to one direction. Filled = upper hemisphere, ring = lower; red operations include time reversal. Lines are mirrors; polygons are 2/3/4/6-fold axes; the centre ring is inversion.

Every structure in C 2′/c′ →
Atom sites · 2 sites · CSV
siteelementxyzmambmc|m| (μB)
Nd1Nd00.1310.252.1700.882.3416
Pt1Pt00.4160.25

Moment components are along the crystal axes a, b, c (μB), as magCIF writes them. Symmetry generates the rest of the cell from these sites.

Source

A. Castets et al. Solid State Communications (1982) · doi:10.1016/0038-1098(82)91116-4

Cite the original paper and MAGNDATA, not this mirror.

Original file

⬇ 0.690_NdPt.mcif from MAGNDATA · entry page