Spin lattice of LaMn2Si2Spin lattice of LaMn2Si2

LaMn2Si2

MAGNDATA entry 0.497 · source
noncollinear ferrimagnet
Opposite moments of different size leave a net magnetisation.
ordered ≤ 310 K (37 °C)Colour: where that sits relative to 25 °C. Saturation: how much margin it has.
Structure · 10 properties
Magnetic groupI m′ m 2′ BNS 44.231
Parent space groupI 4/m m m No. 139
Spinscoplanar · net moment 6.728 μB per cell
Propagation[0 0 0] 1k
Cella 4.0985 · b 4.0985 · c 10.5633 Å · α 90° · β 90° · γ 90°
Transition310 K (37 °C)
Measured at10 K
Magnetic ionsMn
Largest moment component1.993 μB
MethodNPD

Symmetry

Stereogram of the magnetic point group: each operation applied to one direction. Filled = upper hemisphere, ring = lower; red operations include time reversal. Lines are mirrors; polygons are 2/3/4/6-fold axes; the centre ring is inversion.

Every structure in I m′ m 2′ →
Atom sites · 3 sites · CSV
siteelementxyzmambmc|m| (μB)
La1La000
Mn1Mn00.50.25−1.99301.6822.6079
Si1Si000.3801

Moment components are along the crystal axes a, b, c (μB), as magCIF writes them. Symmetry generates the rest of the cell from these sites.

Source

M. Hofmann et al. Materials Science Forum (1996) · doi:10.4028/www.scientific.net/MSF.228-231.587

Cite the original paper and MAGNDATA, not this mirror.

Original file

⬇ 0.497_LaMn2Si2.mcif from MAGNDATA · entry page

sha256 of this copy: e8afc592e61b5e8a9dcc332b99594da69fd845c973800e2a2f74d267c8d04b0e
The mirror keeps the bytes Bilbao served, so the original should hash the same unless MAGNDATA has revised the entry since: shasum -a 256 0.497_LaMn2Si2.mcif.