Research/Sitter/MAGNDATA / 0.388_Co3Al2Si3O12.mcif

⬇ Download .mcif  ·  Data (JSON)

Spin lattice of Co3Al2Si3O12Spin lattice of Co3Al2Si3O12

Co3Al2Si3O12

MAGNDATA entry 0.388 · source
noncoplanar magnet
Spins pointing in three dimensions, not confined to a plane.
ordered ≤ 11 K (−262 °C)Colour: where that sits relative to 25 °C. Saturation: how much margin it has.
Structure · 10 properties
Magnetic groupI 41/a′ c d BNS 142.563
Parent space groupI a 3 d No. 230
Spinsnoncoplanar · net moment 0 μB per cell
Propagation[0 0 0] 1k
Cella 11.4147 · b 11.4147 · c 11.4147 Å · α 90° · β 90° · γ 90°
Transition11 K (−262 °C)
Measured at2 K
Magnetic ionsCo
Largest moment component3.45 μB
MethodNPD

Symmetry

Stereogram of the magnetic point group: each operation applied to one direction. Filled = upper hemisphere, ring = lower; red operations include time reversal. Lines are mirrors; polygons are 2/3/4/6-fold axes; the centre ring is inversion.

Every structure in I 41/a′ c d →
Atom sites · 8 sites · CSV
siteelementxyzmambmc|m| (μB)
Co1_1Co0.12500.253.45003.45
Co1_2Co0.250.12502.8201.993.4514
Al1Al000
Si1_1Si0.37500.25
Si1_2Si0.250.3750
O1_1O0.03360.05170.653
O1_2O0.6530.03360.0517
O1_3O0.05170.6530.0336

Moment components are along the crystal axes a, b, c (μB), as magCIF writes them. Symmetry generates the rest of the cell from these sites.

Source

Q. Cui et al. PHYSICAL REVIEW B (2020) · doi:10.1103/PhysRevB.101.144424

Cite the original paper and MAGNDATA, not this mirror.

Original file

⬇ 0.388_Co3Al2Si3O12.mcif from MAGNDATA · entry page

sha256 of this copy: f17dc287df3389b799e7f6d5a074debfef2135bbf90a599a3e14da966711bbf2