Research/Sitter/MAGNDATA / 0.289_NdMnO3.mcif

⬇ Download .mcif  ·  Data (JSON)

Spin lattice of NdMnO3Spin lattice of NdMnO3

NdMnO3

MAGNDATA entry 0.289 · source
noncollinear ferrimagnet
Opposite moments of different size leave a net magnetisation.
ordered ≤ 13 K (−260 °C)Colour: where that sits relative to 25 °C. Saturation: how much margin it has.
Structure · 10 properties
Magnetic groupP n′ m a′ BNS 62.448
Parent space groupP n m a No. 62
Spinscoplanar · net moment 11.2 μB per cell
Propagation[0 0 0] 1k
Cella 5.7119 · b 7.589 · c 5.4119 Å · α 90° · β 90° · γ 90°
Transition13 K (−260 °C)
Measured at1.5 K
Magnetic ionsMn, Nd
Largest moment component2.8 μB
MethodNPD

Symmetry

Stereogram of the magnetic point group: each operation applied to one direction. Filled = upper hemisphere, ring = lower; red operations include time reversal. Lines are mirrors; polygons are 2/3/4/6-fold axes; the centre ring is inversion.

Every structure in P n′ m a′ →
Atom sites · 4 sites · CSV
siteelementxyzmambmc|m| (μB)
Nd1Nd0.05970.250.99090−1.201.2
Mn1Mn000.52.8−1.603.2249
O1O0.48370.250.0817
O2O0.31060.04050.7108

Moment components are along the crystal axes a, b, c (μB), as magCIF writes them. Symmetry generates the rest of the cell from these sites.

Source

A. Munoz et al. J. Phys.: Condens. Matter (2000) · doi:10.1088/0953-8984/12/7/319

Cite the original paper and MAGNDATA, not this mirror.

Original file

⬇ 0.289_NdMnO3.mcif from MAGNDATA · entry page

sha256 of this copy: d24a5246c46c78e80a7a1e33444b233f5d25678d072fcae455fbabeaeac1e352
The mirror keeps the bytes Bilbao served, so the original should hash the same unless MAGNDATA has revised the entry since: shasum -a 256 0.289_NdMnO3.mcif.