Research/Sitter/MAGNDATA / 0.177_Mn3GaN.mcif

⬇ Download .mcif  ·  Data (JSON)

Spin lattice of Mn3GaNSpin lattice of Mn3GaN

Mn3GaN

MAGNDATA entry 0.177 · source
noncollinear antiferromagnet
All moments add up to a net magnetisation: an ordinary magnet. Spin splitting is the same in every direction (s-wave).
ordered ≤ 298 K (25 °C)Colour: where that sits relative to 25 °C. Saturation: how much margin it has.
Structure · 10 properties
Magnetic groupR3m BNS 166.97
Parent space groupP m3 m No. 221
Spinscoplanar · net moment 0 μB per cell
Propagation[0 0 0] 1k
Cella 3.898 · b 3.898 · c 3.898 Å · α 90° · β 90° · γ 90°
Transition298 K (25 °C)
Measured at4.2 K
Magnetic ionsMn
Largest moment component0.83 μB
MethodND

Symmetry

Stereogram of the magnetic point group: each operation applied to one direction. Filled = upper hemisphere, ring = lower; red operations include time reversal. Lines are mirrors; polygons are 2/3/4/6-fold axes; the centre ring is inversion.

Every structure in R3m →
Atom sites · 3 sites · CSV
siteelementxyzmambmc|m| (μB)
Ga1Ga000
Mn1Mn00.50.500.83−0.831.1738
N1N0.50.50.5

Moment components are along the crystal axes a, b, c (μB), as magCIF writes them. Symmetry generates the rest of the cell from these sites.

Source

D. Fruchart et al. J. Phys. Soc. Jpn (1978) · doi:10.1143/JPSJ.44.781

Cite the original paper and MAGNDATA, not this mirror.

Original file

⬇ 0.177_Mn3GaN.mcif from MAGNDATA · entry page

sha256 of this copy: 91fa7e5ad787d733e241223bfacc0a6f6743216fd5743e8cdb55cea3442bc9a3
The mirror keeps the bytes Bilbao served, so the original should hash the same unless MAGNDATA has revised the entry since: shasum -a 256 0.177_Mn3GaN.mcif.