Research/Sitter/MAGNDATA / 0.1069_Er2CuMn5O12.mcif

⬇ Download .mcif  ·  Data (JSON)

Spin lattice of Er2CuMn5O12Spin lattice of Er2CuMn5O12

Er2CuMn5O12

MAGNDATA entry 0.1069 · source
s-wave ferrimagnet
Opposite moments of different size leave a net magnetisation.
Spin group ¹2/¹m: each symmetry marked ¹ keeps every spin, ² swaps up and down.
ordered ≤ 172 K (−101 °C)Colour: where that sits relative to 25 °C. Saturation: how much margin it has.
Structure · 11 properties
Magnetic groupP m m′ n′ BNS 59.410
Point groupm′m′m
Parent space groupP m m n No. 59
Spinscollinear · net moment 10.06 μB per cell
Propagation[0 0 0] 1k
Cella 7.31474 · b 7.264 · c 7.77047 Å · α 90° · β 90° · γ 90°
Transition172 K (−101 °C)
Measured at140 K
Magnetic ionsMn
Largest moment component2.28 μB
MethodNPD

Symmetry

Stereogram of the magnetic point group: each operation applied to one direction. Filled = upper hemisphere, ring = lower; red operations include time reversal. Lines are mirrors; polygons are 2/3/4/6-fold axes; the centre ring is inversion.

Every structure in P m m′ n′ →
Atom sites · 13 sites · CSV
siteelementxyzmambmc|m| (μB)
Er1Er0.250.750.2215
Er2Er0.250.750.7166
Cu1Cu0.250.250.2692
Mn1Mn0.250.250.2692
Mn2Mn0.250.250.7588−2.15002.15
Cu2Cu0.250.250.7588
Mn3Mn0002.28−0.1902.2879
Mn4Mn000.51.31001.31
O1O0.43760.06120.2669
O2O0.250.5587−0.0413
O3O0.03350.25−0.0782
O4O0.250.03430.5812
O5O−0.06470.250.5414

Moment components are along the crystal axes a, b, c (μB), as magCIF writes them. Symmetry generates the rest of the cell from these sites.

Source

John M. Attah-Baah et al. Acta Cryst. B (2024) · doi:10.1107/S2052520624008965

Cite the original paper and MAGNDATA, not this mirror.

Original file

⬇ 0.1069_Er2CuMn5O12.mcif from MAGNDATA · entry page

sha256 of this copy: 8797a41c89c7df5a509c58284a10330ced98d6ee676dd0e9fb7b7a4e034528a0
The mirror keeps the bytes Bilbao served, so the original should hash the same unless MAGNDATA has revised the entry since: shasum -a 256 0.1069_Er2CuMn5O12.mcif.